1. Post Mosaic 300*300 visible separation

Reasons: 1) paper shrinkage;

2) the problem of static color;

3) bad seam placement.

2. Mosaic anti-bottom phenomenon

Reason: cement color problem.

Glass Mosaic such as Water Jet Glass Mosaic itself has transparent or translucent characteristics, so the topmost layer needs to choose white cement, to avoid the phenomenon of black cement.

3. After Mosaic paste cracking phenomenon

Reasons: 1) mosaics themselves are too brittle;

2) construction is too hard.

4. The mosaics don't match

Reasons: 1) disclosure of stickers;

2) pre-factory test.

5. After Mosaic paste paper phenomenon

Reasons: 1) the base was not adequately wetted before construction;

2) touch seam not serious.

Square O Water Jet Glass Mosaic


Square O Water Jet Glass Mosaic

6. Mosaic paste found empty drum phenomenon

Reasons: 1) the base empty drum was not inspected, the base cleaning is not clean;

2) the base is not adequately wetted before construction;

3) cement paste is not full and uneven;

4) no iron wipe after the bricks are pasted on the wall;

The beat is firm or uneven.

7. After Mosaic paste uneven phenomenon

Reasons: 1) the flatness of the base was not checked;

2) the construction base paste mud layer is too thick, the base ash is not flat enough, paste cement paste thickness is not uniform;

3) no iron trowel evenly beat solid.

8. Mosaic paste after stagger phenomenon

Reasons: 1) there is no good seaming before construction;

2) no good seam alignment during construction;

3) the construction method of beating paper before paper removal is wrong;

4) paper shrinkage;

5) loose control during laying, not properly sewn and not seamed after peeling the paper.

9. Dirty walls

Reasons: 1) after uncovering the paper, the residual paper wool and paste cement slurry are not cleaned in time;